23 January 2017 J-integral for interface crack on micro-arc oxidation ceramic coating
Author Affiliations +
Proceedings Volume 10322, Seventh International Conference on Electronics and Information Engineering; 1032238 (2017) https://doi.org/10.1117/12.2265237
Event: Seventh International Conference on Electronics and Information Engineering, 2016, Nanjing, China
Abstract
By use of extended finite element analysis method, a calculation of J-integral for interface crack on Micro-arc Oxidation(MAO) ceramic coating on aluminum alloy was conducted. The feasibility of using J-integral as a fracture parameter to characterize the interfacial fracture toughness is discussed. The relation between J-integral and length of interface crack, thickness of ceramic coating is studied. Analysis result indicates that with the expansion of the interface crack length, resistance bi-material interface enhancements, and interfacial fracture toughness enhances, the J-integral increases with the increase of crack length. When the thickness of the ceramic coating is upon 40μm-100μm, interfacial fracture toughness is better. J-integral value shows a decreasing trend with the increase of the thickness of the ceramic coating.
© (2017) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Cheng Gao, Cheng Gao, Huiyu Tao, Huiyu Tao, Dayong Cai, Dayong Cai, Jinyong Xu, Jinyong Xu, Yan Tang, Yan Tang, Ranran Huang, Ranran Huang, } "J-integral for interface crack on micro-arc oxidation ceramic coating", Proc. SPIE 10322, Seventh International Conference on Electronics and Information Engineering, 1032238 (23 January 2017); doi: 10.1117/12.2265237; https://doi.org/10.1117/12.2265237