Abstract
Optical polishing method of large diameter KDP crystals was developed. The surface finishing of KDP crystals was conducted using specially prepared lapping plate and sluny of diamond powder in oil. The optical flatness and the surface roughness of optically polished KDP crystal (2O9mm'x16mmt) were about X/6 and 7- 10 Arms, respectively. The surface damage threshold of about 10 J/cm2 at 1064nm with a pulsewidth of ins was obtained. Key words : laser damage, KDP crystal, optical flatness, surface roughness
© (1992) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Kunio Yoshida, Hidetsugu Yoshida, Sadao Nakai, Yoshimasa Katori, and Takayuki Okamoto "Laser damage of optically polished KDP crystal", Proc. SPIE 1624, Laser-Induced Damage in Optical Materials: 1991, (29 July 1992); https://doi.org/10.1117/12.60123
Lens.org Logo
CITATIONS
Cited by 3 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Crystal optics

Crystals

Polishing

Laser induced damage

Laser crystals

Antireflective coatings

Surface finishing

Back to Top