22 April 1996 Improved processing for silver halide pulse holography
Author Affiliations +
Abstract
Using of an improved developer with optical latensification allowed to significantly increase exposure sensitivity of currently in use silver halide materials. Transmission large-scale holograms (30 X 40 cm2) of diffused objects have been recorded under pulse exposure of about 6.5 X 10-6 J/cm2 for VRP and of about 2 X 10-6 J/cm2 for Agfa-Gavaert 8E56HD, in both cases without appreciable contrast deterioration. Results of the first experiments on pulse reflection holography are also discussed.
© (1996) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Viktor Nikolaevic Mikhailov, Viktor Nikolaevic Mikhailov, Jung-Young Son, Jung-Young Son, Olga V. Grinevitskaya, Olga V. Grinevitskaya, Hyuk-Soo Lee, Hyuk-Soo Lee, Yong-Jin Choi, Yong-Jin Choi, } "Improved processing for silver halide pulse holography", Proc. SPIE 2688, Holographic Materials II, (22 April 1996); doi: 10.1117/12.238541; https://doi.org/10.1117/12.238541
PROCEEDINGS
6 PAGES


SHARE
RELATED CONTENT

Contact Copying Of Holographic Transmission Gratings.
Proceedings of SPIE (March 31 1989)
The Role Of Silver Halide Materials In The Formation Of...
Proceedings of SPIE (August 12 1985)
Pseudo Color Reflection Holography An Artist's...
Proceedings of SPIE (June 04 1987)
Single-layer color hologram recording
Proceedings of SPIE (March 26 1998)
Some new developments in display holography
Proceedings of SPIE (February 01 1991)
Holographic materials available from Geola
Proceedings of SPIE (June 04 2001)

Back to Top