7 September 2001 Measurement of absorption and scattering properties of CVD diamond
Author Affiliations +
Abstract
Temperature dependent infrared transmittance measurements and room temperature BSDF measurements are collected on 1.5mm thick CVD diamond samples produced by De Beers Industrial Diamond Division. The transmittance measurements are from 2 to 20 micrometers covering the temperature range from room temperature to 400 degree(s)C. The BSDF measurements are conducted at wavelengths of 0.6328, 3.39, and 11 micrometers and as a function of the incidence angle. The total integrated scatter is obtained by integrating the BSDF function over all the reflection angles.
© (2001) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Michael E. Thomas, Michael E. Thomas, William J. Green, William J. Green, Di Yang, Di Yang, David W. Blodgett, David W. Blodgett, "Measurement of absorption and scattering properties of CVD diamond", Proc. SPIE 4375, Window and Dome Technologies and Materials VII, (7 September 2001); doi: 10.1117/12.439178; https://doi.org/10.1117/12.439178
PROCEEDINGS
6 PAGES


SHARE
RELATED CONTENT

Temperature dependence of absorption in CVD diamond
Proceedings of SPIE (September 27 1994)
Development of ZnSe Infrared Optical Fiber
Proceedings of SPIE (May 11 1986)
Scattering and absorption of CVD diamond windows
Proceedings of SPIE (December 13 1992)
Optical properties of human whole blood changes due to...
Proceedings of SPIE (December 04 1996)

Back to Top