10 June 2004 ArF-laser-induced photochemical super mirror-finishing of Si wafer (Abstract Only)
Author Affiliations +
Abstract
Si wafer was polished accurately with ArF laser irradiation in the presence of the hydrofluoric acid water solution. The highest surface accuracy of Si wafer is needed for the Si substrate for using extremely ultra violet (EUV) lithography. Then we tried to polish the SiO2 with hydrofluoric acid water solution, which was photo-oxidized Si wafer surface with active oxygen. The active oxygen was photo-dissociated from water (H2O). The Si wafer surface was pressurized at 50g/cm2 on the fluorocarbon-polishing mat. Next the hydrofluoric acid water solution is infiltrated into the thin gap between the sample and the fluorocarbon. And ArF laser is irradiated through the fluorocarbon turntable. By this irradiation, the Si wafer surface was oxidized and produced SiO2. The moment it is dissolved by HF solution. After the etching, the polishing progresses by the friction with the fluorocarbon. The surface roughness was obtained 3 nm with 30 minute polishing with the ArF laser irradiation (20 mJ/cm2, 100 pps) in 15% HF/H2O ambience.
© (2004) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Masataka M. Murahara "ArF-laser-induced photochemical super mirror-finishing of Si wafer (Abstract Only)", Proc. SPIE 5273, Laser-Induced Damage in Optical Materials: 2003, (10 June 2004); https://doi.org/10.1117/12.524848
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Silicon

Semiconducting wafers

Polishing

Surface finishing

Chemical lasers

Laser irradiation

Oxygen

RELATED CONTENT

Model-based control of chemical mechanical polishing
Proceedings of SPIE (August 25 1997)
Optoelectronic properties of ion-etched silicon surfaces
Proceedings of SPIE (April 22 2008)
The role of defects in the laser desorption of ions...
Proceedings of SPIE (April 25 2007)
Damage-free grinding using ultrafine abrasives
Proceedings of SPIE (October 01 1990)
Fabrication of EUV components with MRF
Proceedings of SPIE (January 13 2004)
A comparative study and optimal choice of the method of...
Proceedings of SPIE (September 30 2003)

Back to Top