28 April 2006 Comparison of various optical characterization techniques for the surface analysis of optical-grade germanium infrared materials
Author Affiliations +
Abstract
Optimization of the optical quality of optical-grade germanium components requires an in-depth investigation of the different contributions to the optical loss in germanium. In this paper we therefore focus on this optical characterization. We give an overview of possible characterization techniques to determine surface roughness, surface/bulk absorption and refractive index inhomogeneities and we highlight the obtained optical characteristics. To conclude we select the most appropriate non-destructive characterization tool for each optical parameter.
© (2006) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Heidi Ottevaere, Heidi Ottevaere, Anna Szpak, Anna Szpak, Igor Romandic, Igor Romandic, Jan Van Nylen, Jan Van Nylen, Hans Vercammen, Hans Vercammen, Dirk Vyncke, Dirk Vyncke, Malgorzata Kujawinska, Malgorzata Kujawinska, Hugo Thienpont, Hugo Thienpont, } "Comparison of various optical characterization techniques for the surface analysis of optical-grade germanium infrared materials", Proc. SPIE 6188, Optical Micro- and Nanometrology in Microsystems Technology, 61881D (28 April 2006); doi: 10.1117/12.663598; https://doi.org/10.1117/12.663598
PROCEEDINGS
10 PAGES


SHARE
Back to Top