Contact holes represent one of the biggest critical dimension (CD) mask metrology challenges for 45nm technology mask development. The challenge is a consequence of both wafer and mask sensitivities. Large mask error factors and the small process windows found when contact holes are imaged on wafers impose very tight mask specifications for CD uniformity. The resultant CD error budget leaves little room for mask metrology. Current advanced mask metrology deploys a CD-SEM to characterize the mask contact hole CD uniformity. Measuring a contact hole is complex since it is inherently two-dimensional and is not always well-characterized by one-dimensional x- and y-axis measurements. This paper will investigate contact metrics such as line edge roughness (LER), region of interest (ROI) size, area, and CD sampling methods. The relative merits of each will be explored. Ultimately, an understanding of the connection between what is physically measured on the mask and what impacts wafer imaging must be understood. Simulations will be presented to explore the printability of a contact hole's physical attributes. The results will be summarized into a discussion of optimal contact hole metrology for 45nm technology node masks.
© (2006) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Masaru Higuchi, Emily Gallagher, Daniel Ceperley, Timothy Brunner, Reg Bowley, and Anne McGuire "Revisiting mask contact hole measurements", Proc. SPIE 6349, Photomask Technology 2006, 634947 (20 October 2006); https://doi.org/10.1117/12.686957
Lens.org Logo
CITATIONS
Cited by 3 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Photomasks

Semiconducting wafers

Metrology

Line edge roughness

Critical dimension metrology

Error analysis

Time metrology

RELATED CONTENT

ACLV performance dry vs. immersion on 45-nm ground rules
Proceedings of SPIE (March 27 2007)
Aerial imaging for FABs: productivity and yield aspects
Proceedings of SPIE (March 23 2009)
Exploring the sources of MEEF in contact SRAMs
Proceedings of SPIE (October 30 2007)
Metrology qualification of EUV resists
Proceedings of SPIE (April 15 2010)
CD-SEM suitability for CD metrology of modern photomasks
Proceedings of SPIE (August 25 1999)

Back to Top