27 November 2007 Investigation on addition of TiB2 on sintering behavior and mechanical properties of B4C
H. Abdizadeh, H. R. Baharvandi, A. M. Hadian, N. Ehsani
Author Affiliations +
Proceedings Volume 6423, International Conference on Smart Materials and Nanotechnology in Engineering; 64233B (2007) https://doi.org/10.1117/12.780018
Event: International Conference on Smart Materials and Nanotechnology in Engineering, 2007, Harbin, China
Abstract
The objective of the present investigation was to study the effect of TiB2 addition on sintering behavior and mechanical properties of pressureless-sintered B4C ceramic. Different amounts of TiB2, mainly 5 to 30wt% were added to the base material. Addition of 30wt% TiB2 and sintering at 2050°C resulted in improving the density of the samples to about 98.5% of the theoretical density. The composite samples exhibited very good mechanical properties (hardness, flexural strength and fracture toughness). As the amount of TiB2 was increased from 15 to 30, the mechanical properties were reduced, except for the fracture toughness, apparently due to excess amount of sintering aid in the specimen.
© (2007) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
H. Abdizadeh, H. R. Baharvandi, A. M. Hadian, and N. Ehsani "Investigation on addition of TiB2 on sintering behavior and mechanical properties of B4C", Proc. SPIE 6423, International Conference on Smart Materials and Nanotechnology in Engineering, 64233B (27 November 2007); https://doi.org/10.1117/12.780018
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Boron

Composites

Ceramics

Polishing

Scanning electron microscopy

Surface finishing

Aluminum

Back to Top