31 December 2008 Formation of two side-direction burr in grinding-hardening machining
Judong Liu, Guicheng Wang, Dapan Hou, Zhilong Xu
Author Affiliations +
Proceedings Volume 7130, Fourth International Symposium on Precision Mechanical Measurements; 71305U (2008) https://doi.org/10.1117/12.819770
Event: Fourth International Symposium on Precision Mechanical Measurements, 2008, Anhui, China
Abstract
Based on the surface grind hardening experiment, major forms of two side-direction burr are given out through the experimental observation, as well as its formation and variations are studied. The studies show that in the processes of the grinding-hardening, metal in the vicinity to the contact region under the high temperature plastic flows toward the free surface without constraints in two sides so to form the two side-direction burr, under the action of an abrasive wheel. The morphology and size of two side-direction burr varies with changes of the grinding conditions. The higher the grinding temperature is, then the larger the grinding force is, and the bigger the size of the two side-direction burr is.
© (2008) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Judong Liu, Guicheng Wang, Dapan Hou, and Zhilong Xu "Formation of two side-direction burr in grinding-hardening machining", Proc. SPIE 7130, Fourth International Symposium on Precision Mechanical Measurements, 71305U (31 December 2008); https://doi.org/10.1117/12.819770
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Abrasives

Metals

Surface finishing

Heat treatments

Polishing

Classification systems

Diamond

Back to Top