Abstract
Laser metal deposition (LMD) with high power lasers consists of manufacturing precise layers of materials by fusing metal powder with a laser beam over a substrate. Typical dilution of 5% allows metallurgical adhesion of the coating. This technique provides a unique combination of high accuracy and low heat affecting zone which is attractive for processing high added value components such aeroengines. Nickel (Ni) base superalloys are widely used in aeroengines because of their high mechanical properties when working at high temperatures (creep). A repairing or manufacturing chain of these components by LMD requires a good understanding of many parameters; therefore process control plays an important role. This work is focused on the study of the LMD processing of a Ni base superalloy using two colour pyrometry for the process monitoring. Presented results show how temperature and cooling rates of the LMD tracks affect the shape, microstructure and corrosion of the LMD coatings.
© (2010) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Bernabe Carcel, Bernabe Carcel, Jesus Sampedro, Jesus Sampedro, Irene Perez, Irene Perez, Estrella Fernandez, Estrella Fernandez, Jose A. Ramos, Jose A. Ramos, "Improved laser metal deposition (LMD) of nickel base superalloys by pyrometry process control", Proc. SPIE 7751, XVIII International Symposium on Gas Flow, Chemical Lasers, and High-Power Lasers, 775123 (16 November 2010); doi: 10.1117/12.878749; https://doi.org/10.1117/12.878749
PROCEEDINGS
9 PAGES


SHARE
RELATED CONTENT

Laser-assisted micro sheet forming
Proceedings of SPIE (January 14 2008)
Experimental investigations in laser microsoldering
Proceedings of SPIE (November 30 1991)
State of the art in bipolar of proton exchange membrane...
Proceedings of SPIE (October 12 2010)
Developments in CD-R
Proceedings of SPIE (February 06 2001)
Sensors for material process monitoring and control
Proceedings of SPIE (October 03 1995)

Back to Top