The results of quantum-chemical analysis of elastic and strength properties of the bamboo-like tube are presented in this paper. For the first time the configuration of the thinnest stable bamboo-like tube was established. The bamboo-like nanotube breaking point is established to be under compression of 11GPa. Configuration of the nanoindentor based on symmetric and streamlined tip of the tube (15,15), presented in this work, provides perfect interaction between the nanoindentor tip and the tissue because tip has no sharp protruding pieces.
© (2012) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
O. E. Glukhova, A. S. Kolesnikova, E. L. Kossovich, and R. Y. Zhnichkov "Super strong nanoindentors for biomedical applications based on bamboo-like nanotubes", Proc. SPIE 8233, Reporters, Markers, Dyes, Nanoparticles, and Molecular Probes for Biomedical Applications IV, 823311 (2 February 2012); https://doi.org/10.1117/12.907035
PROCEEDINGS
8 PAGES


SHARE
Advertisement
Advertisement
Back to Top