You have requested a machine translation of selected content from our databases. This functionality is provided solely for your convenience and is in no way intended to replace human translation. Neither SPIE nor the owners and publishers of the content make, and they explicitly disclaim, any express or implied representations or warranties of any kind, including, without limitation, representations and warranties as to the functionality of the translation feature or the accuracy or completeness of the translations.
Translations are not retained in our system. Your use of this feature and the translations is subject to all use restrictions contained in the Terms and Conditions of Use of the SPIE website.
3 December 2015Simulation on the steel galvanic corrosion and acoustic emission
Galvanic corrosion is a very destructive localized corrosion. The research on galvanic corrosion could determine equipment corrosion and prevent the accidents occurrence. Steel corrosion had been studied by COMSOL software with mathematical modeling. The galvanic corrosion of steel-aluminum submerged into 10% sodium chloride solution had been on-line detected by PIC-2 acoustic emission system. The results show that the acoustic emission event counts detected within unit time can qualitative judge galvanic corrosion rate and further erosion trend can be judged by the value changes.
Yang Yu,Xin Shi, andPing Yang
"Simulation on the steel galvanic corrosion and acoustic emission", Proc. SPIE 9794, Sixth International Conference on Electronics and Information Engineering, 97942E (3 December 2015); https://doi.org/10.1117/12.2202387
The alert did not successfully save. Please try again later.
Yang Yu, Xin Shi, Ping Yang, "Simulation on the steel galvanic corrosion and acoustic emission," Proc. SPIE 9794, Sixth International Conference on Electronics and Information Engineering, 97942E (3 December 2015); https://doi.org/10.1117/12.2202387