1 October 1993 Process techniques for improving performance of positive tone silylation
Author Affiliations +
Optical Engineering, 32(10), (1993). doi:10.1117/12.146858
Abstract
Two approaches that control the overflow of silylated material that can occur subsequent to surface imaging of acid-hardened resists are introduced. Treatment of the resist surface with a cross-linking agent [bis(dimethylamino)dimethylsilane] prior to silylation can produce a surface layer with the physical integrity to constrain silylated material. Alternatively, the unexposed areas of the resist may be partially removed by development with a basic solution. The surface depressions thus produced allow volume expansion to occur during silylation without causing overflow.
Edward K. Pavelchek, Gary S. Calabrese, John F. Bohland, Bruce W. Dudley, Susan K. Jones, Peter W. Freeman, "Process techniques for improving performance of positive tone silylation," Optical Engineering 32(10), (1 October 1993). https://doi.org/10.1117/12.146858
JOURNAL ARTICLE
6 PAGES


SHARE
Back to Top