9 March 2018 Berkovich nanoindentation of borosilicate K9 glass
Chenghui Gao, Ligang Yao, Ming Liu
Author Affiliations +
Abstract
Instrumented indentation was used to investigate the proportional relationships among indentation variables such as the maximum indentation displacement, contact depth, the ratio of load over contact stiffness, and the ratio of permanent displacement over the maximum displacement. Material and indenter were borosilicate K9 glass and a Berkovich indenter, respectively. Results of fused silica under the same indenter were compared. Load–displacement curves of K9 glass were characterized by power-law functions for both loading (power exponent of 2) and unloading (power exponent of 1.36) with hardness, elastic modulus, yield stress, and power strain hardening exponent being 7.72, 82.8, 3.5 GPa, and 0.6, respectively. Experimental results were found to be in agreement with theoretical prediction and dimensional analysis. The results calculated from energy-based method were found to be consistent with those based on Oliver and Pharr’s method. General implications of the scaling relations for indentation variables were discussed (e.g., the scaling expressions can be used to check indentation data).
© 2018 Society of Photo-Optical Instrumentation Engineers (SPIE) 0091-3286/2018/$25.00 © 2018 SPIE
Chenghui Gao, Ligang Yao, and Ming Liu "Berkovich nanoindentation of borosilicate K9 glass," Optical Engineering 57(3), 034104 (9 March 2018). https://doi.org/10.1117/1.OE.57.3.034104
Received: 27 November 2017; Accepted: 15 February 2018; Published: 9 March 2018
Lens.org Logo
CITATIONS
Cited by 19 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Glasses

Information technology

Silica

Optical engineering

Spherical lenses

Calibration

Commercial off the shelf technology

RELATED CONTENT

A piezoelectric shear stress sensor
Proceedings of SPIE (April 20 2016)
A simple ball averager for reference sphere calibrations
Proceedings of SPIE (August 19 2005)
Controlling nonlinearities in elastic actuators
Proceedings of SPIE (September 06 1995)

Back to Top